FIBERGLASS TISSUE

 

FIBERGLASS SURFACE TISSUE

The surface tissue is mainly used in the surface layers of FRP products at Hand lay up or filament winding, pultrusion process etc.

Weight (g/m2)
23
30
40
50
60
Binder Content (%)
6-9
Soaking time (s) two layer
8
10
13
16
20
Tensile strength MD N/50mm
35
40
50
60
70
Moisture Content (%)
<= 0.50
Width (mm)
< 1300 (according to request)
Roll Length (m)
According to request

 

FIBERGLASS INNER WARP TISSUE

The inner warp tissue is mainly used as based materials for anti-corrosion warpping on steel pipelines for oil or gas transportation.

Weight (g/m2)
50
60
90
Binder Content (%)
< 20
Tensile strength CD N/50mm
> 75
> 90
> 140
Tensile strength MD N/50mm
> 200
> 220
> 280
Tear Strength MD (g)
> 100
Thickness (mm)
> 0.33
> 0.33
> 0.40
Penetration Pa
5.5 - 18.9
Moisture Content (%)
< 1.0

 

FIBERGLASS ROOFING TISSUE

The roofing tissue is used as excellent substrates for water-proof materials.

Weight (g/m2)
50
60
90
50
60
90
Binder Content (%)
< 25
Space between yarns
/
/
/
12
12
12
Tensile strength CD N/50mm
120
150
230
85
130
210
Tensile strength MD N/50mm
210
230
330
230
240
350
Wet strength N/50mm
70
80
110
80
80
115

 